Balance Community Materials test laboratory · SnapLab

Record Sample 3
Product Axiom MK2
Batch W26DZ-2

Tensile test

Sample 3

Axiom MK2Batch W26DZ-2October 15, 2026

Breaking force

49.41kN

Force–time trace

The capture from the rig’s force channel, plotted against elapsed time. Zoom or drag to load the full-resolution record.

Test details

Tested
Oct 15, 2026 · 14:50
Duration
133.2s
Scan rate
500Hz
Sample
3
Study
Batch Report - Axiom MK2 - W26DZ-2
Test machine
SnapLab break-test bench
DAQ device
LabJack T7
Beam location
No. 2 — Second position

Instrumentation

Recorded channels
Channel Sensor Type Units Calibrated
AIN2 Main Main Force Sensor force kN Not recorded

Method

Configuration Sewn Loop to Sewn Loop

Sewing pattern Diamond ramp for 20 mm webbings Pattern 504

Determines strength retention in a sewn loop. The particular pattern used for sewing is indicated on each test.

Each sewn loop is done in an opposite direction in order to take out the possibility of failure by uneven loading across the width and thickness of the webbing. Each sewn loop is directly attached to the clevis pins on our test machine, with a diameter of pin diameter of 19mm.

These tests are often used as our elongation tests as well, since they experience the least change in length within the anchoring method.

  • Webbing starting length - 1.5 m (5 ft)

  • Pull Rate - ~350 mm per minute

Part of batch W26DZ-2 →